Main navigation
Specially designed for you, this tool will help you estimate, step by step, the thickness of the coating to apply and the quantity fo wire to use in all your projects, whichever corrosion classes you work with and the type of wire selected.
* The figure given above is purely theoretical and is given for information only. It therefore does not engage Zinacor S.A. in any way. In practice, you will have to take into account many technical, design and human factors that will increase the quantity to be used.
Get in touch helps us to understand you better
Rue de Chênée 53 (entrée B)
B-4031 Angleur- Belgique
Telephone +3243666471
Get in touch helps us to understand you better
- Technical advices
-
Too rough metal coated surface
Too rough metal coated surface
Possible causes:
- too low gas pressure: increase pressure;
- too large wire diameter: reduce the diameter;
- nozzles are not ideal: replace the nozzles.
Other questions
-
Category :Electric arc spray gun : the wire does not come out
-
Category :Flame spray gun : the wire is stuck inside the gun
-
Category :Poor coating adhesion
ISO 2063 Standard
Contact
We use cookies to improve your online experience.
For more information, visit our privacy policy